The controversial role of inter-diffusion in glass alteration
S Gin, L Neill, M Fournier, P Frugier, T Ducasse, M Tribet, A Abdelouas, ...
Chemical Geology 440, 115-123, 2016
1022016
Long-term alteration of basaltic glass: Mechanisms and rates
B Parruzot, P Jollivet, D Rébiscoul, S Gin
Geochimica et Cosmochimica Acta 154, 28-48, 2015
842015
The dissolution behavior of borosilicate glasses in far-from equilibrium conditions
JJ Neeway, PC Rieke, BP Parruzot, JV Ryan, RM Asmussen
Geochimica et Cosmochimica Acta 226, 132-148, 2018
512018
Effects of Al: Si and (Al+ Na): Si ratios on the properties of the international simple glass, part II: Structure
X Lu, JT Reiser, B Parruzot, L Deng, IM Gussev, JC Neuefeind, ...
Journal of the American Ceramic Society 104 (1), 183-207, 2021
302021
Acceleration of glass alteration rates induced by zeolite seeds at controlled pH
JJ Neeway, BP Parruzot, JF Bonnett, JT Reiser, SN Kerisit, JV Ryan, ...
Applied Geochemistry 113, 104515, 2020
212020
The use of positrons to survey alteration layers on synthetic nuclear waste glasses
JT Reiser, B Parruzot, MH Weber, JV Ryan, JS McCloy, NA Wall
Journal of Nuclear Materials 490, 75-84, 2017
212017
Effects of Al: Si and (Al+ Na): Si ratios on the properties of the international simple glass, part I: Physical properties
JT Reiser, X Lu, B Parruzot, H Liu, T Subramani, H Kaya, RM Kissinger, ...
Journal of the American Ceramic Society 104 (1), 167-182, 2021
202021
Multi-glass investigation of Stage III glass dissolution behavior from 22 to 90° C triggered by the addition of zeolite phases
B Parruzot, JV Ryan, JL George, RK Motkuri, JF Bonnett, LM Seymour, ...
Journal of Nuclear Materials 523, 490-501, 2019
182019
Effects of Al: Si and (Al+ Na): Si ratios on the static corrosion of sodium‐boroaluminosilicate glasses
JT Reiser, B Parruzot, S Gin, JF Bonnett, CS Smoljan, LM Seymour, ...
International Journal of Applied Glass Science 13 (1), 94-111, 2022
152022
In-situ monitoring of seeded and unseeded stage III corrosion using Raman spectroscopy
JV Ryan, B Parruzot, AM Lines, SA Bryan, LM Seymour, JF Bonnett, ...
npj Materials Degradation 3 (1), 34, 2019
142019
Seeded Stage III glass dissolution behavior of a statistically designed glass matrix
JV Crum, JT Reiser, BP Parruzot, JJ Neeway, JF Bonnett, SN Kerisit, ...
Journal of the American Ceramic Society 104 (8), 4145-4162, 2021
112021
Glass corrosion in the presence of iron-bearing materials and potential corrosion suppressors
J Reiser, L Neill, J Weaver, B Parruzot, C Musa, J Neeway, J Ryan, ...
MRS Online Proceedings Library (OPL) 1744, 139-144, 2015
112015
Effect of zeolite type, temperature, and pH on Stage III glass alteration behavior for two nuclear waste glasses
B Parruzot, JV Crum, JT Reiser, JJ Neeway, SN Kerisit, RC Daniel, ...
Journal of Nuclear Materials 567, 153717, 2022
102022
Vanadium Oxidation States and Structural Role in Aluminoborosilicate Glasses: An Integrated Experimental and Molecular Dynamics Simulation Study
X Lu, L Deng, SA Saslow, H Liu, CJ Benmore, BP Parruzot, JT Reiser, ...
The Journal of Physical Chemistry B 125 (44), 12365-12377, 2021
102021
Method for the in situ measurement of pH and alteration extent for aluminoborosilicate glasses using Raman spectroscopy
B Parruzot, JV Ryan, AM Lines, SA Bryan, JJ Neeway, S Chatterjee, ...
Analytical chemistry 90 (20), 11812-11819, 2018
102018
Altération des verres basaltiques dans des environnements confinés: Analogie avec le stockage géologique des verres nucléaires
B Parruzot
Montpellier 2, 2014
10*2014
Product Consistency Test and Vapor Hydration Test Comparisons of a Radioactive Hanford Waste Glass with its Non-Radioactive Simulant Glass
JTG Reiser, JJ Neeway, BPG Parruzot, E Cordova, SK Cooley, JD Vienna
Pacific Northwest National Laboratory (PNNL), Richland, WA (United States), 2023
52023
Compositional dependence of crystallization and chemical durability in alkali aluminoborosilicate glasses
A Deshkar, B Parruzot, RE Youngman, O Gulbiten, JD Vienna, A Goel
Journal of Non-Crystalline Solids 590, 121694, 2022
52022
GeoMeltR In-Container Vitrification (ICV)TM for Fukushima Daiichi Water Treatment Secondary Wastes - 20212
KG Finucane, BE Campbell, BPG Parruzot, JTG Reiser, JD Vienna
3
Effect of composition on the corrosion behavior of 24 statistically-designed alkali-borosilicate waste glasses
JJ Neeway, JT Reiser, SN Kerisit, RA Reyes, RC Daniel, GL Smith, ...
Journal of Nuclear Materials 586, 154674, 2023
22023